Base Resin Density 0.956 g/cc
0.0345 lb/in³
ASTM D1505
Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene
HB6200 is a high density polyethylene for blow molding. HB6200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applic..