Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.956 g/cc | 0.0345 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene HB6200 is a high density polyethylene for blow molding. HB6200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applic.. |