Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 4.0 g/10 min | 4.0 g/10 min | I<sub>2</sub>; ASTM D1238 |
Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin
(discontinued **) MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excelle.. |
|||
Base Resin Melt Index | 4.0 g/10 min @Temperature 230 °C |
4.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju.. |
|||
Base Resin Melt Index | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANZEX® HI2200 High density polyethylene HI2200 is a high density polyethylene for injection molding. HI2200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a.Ap.. |