Linear Mold Shrinkage 0.002 - 0.003 cm/cm
0.002 - 0.003 in/in
ASTM D955
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
Linear Mold Shrinkage 0.002 cm/cm
0.002 in/in
ASTM D955
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole
RXÂ 640 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.Information supp..
Linear Mold Shrinkage 0.002 - 0.004 cm/cm
0.002 - 0.004 in/in
Compression Molding; ASTM D955
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound
Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information ..