Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.002 - 0.004 cm/cm | 0.002 - 0.004 in/in | Compression Molding; ASTM D955 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |