Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00233 - 0.0101 cm/cm | 0.00233 - 0.0101 in/in | Average value: 0.00554 cm/cm Grade Count:10 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00233 cm/cm | 0.00233 in/in | ASTM D955 |
Plenco 6582 Phenolic, Briquette, Injection Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Linear Mold Shrinkage | 0.00233 cm/cm | 0.00233 in/in | ASTM D955 |
Plenco 7507 Phenolic, Granular, Transfer Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |