Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Glass Filled
Manufacturer Covestro
Trade Name Baydur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.25 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 0.580 g/cc
0.0210 lb/in³
ASTM D792
Apparent Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0024 cm/cm
0.0024 in/in
Bayer Test
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ASTM D2240
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D638/D412
Elongation at Break 11 %
11 %
ASTM D638/D412
Flexural Yield Strength 37.0 MPa
5370 psi
ASTM D790
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
Izod Impact, Unnotched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 49.0 °C
120 °F
ASTM D648