Physical Properties Metric English Comments
Linear Mold Shrinkage 0.004 - 0.007 cm/cm
0.004 - 0.007 in/in
ASTM D955
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.004 - 0.006 cm/cm
0.004 - 0.006 in/in
ASTM D955
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.004 - 0.006 cm/cm
0.004 - 0.006 in/in
ASTM D955
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized
Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.004 - 0.007 cm/cm
0.004 - 0.007 in/in
ASTM D955
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).