Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | ASTM D955 |
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.004 - 0.007 cm/cm | 0.004 - 0.007 in/in | ASTM D955 |
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.004 - 0.007 cm/cm | 0.004 - 0.007 in/in | ASTM D955 |
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | ASTM D955 |
Entec Hylex® P1310L1 HB Polycarbonate Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | ASTM D955 |
Entec Hylex® P1307L1 HB Polycarbonate UV Stabilized, Low Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | ASTM D955 |
Entec Hylex® P1317L1 HB Polycarbonate UV Stabilized, Higher Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | ASTM D955 |
Entec Hylex® P1325L1 HB Polycarbonate UV Stabilized, High Flow, Mold Release, Water ClearInformation provided by Entec. |