Physical Properties Metric English Comments
Linear Mold Shrinkage 0.005 - 0.007 cm/cm
0.005 - 0.007 in/in
ASTM D955
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.004 - 0.007 cm/cm
0.004 - 0.007 in/in
ASTM D955
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.004 - 0.007 cm/cm
0.004 - 0.007 in/in
ASTM D955
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage 0.005 - 0.007 cm/cm
0.005 - 0.007 in/in
ASTM D955
Entec Hylex® P1310L1 HB Polycarbonate
Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release, Water ClearInformation provided by Entec.
Linear Mold Shrinkage 0.005 - 0.007 cm/cm
0.005 - 0.007 in/in
ASTM D955
Entec Hylex® P1307L1 HB Polycarbonate
UV Stabilized, Low Flow, Mold Release, Water ClearInformation provided by Entec.
Linear Mold Shrinkage 0.005 - 0.007 cm/cm
0.005 - 0.007 in/in
ASTM D955
Entec Hylex® P1317L1 HB Polycarbonate
UV Stabilized, Higher Flow, Mold Release, Water ClearInformation provided by Entec.
Linear Mold Shrinkage 0.005 - 0.007 cm/cm
0.005 - 0.007 in/in
ASTM D955
Entec Hylex® P1325L1 HB Polycarbonate
UV Stabilized, High Flow, Mold Release, Water ClearInformation provided by Entec.