Polymer Property : Linear Mold Shrinkage = 0.0082 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
STN 64 0808
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
STN 64 0808
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre
FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling
FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
Isotropy
Solvay TECHNYL® A 221 Natural FA PA66, DRY
Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
Isotropy
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
ASTM D955
SK Chemicals SKYTHANE® S175A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
ASTM D955
Plenco 3356 Phenolic, Granular, Injection Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
ASTM D955
Plenco 4599 Phenolic, Granular, Injection Molded
PLENCO 04599 is a mineral filled, phenolic molding compound offering excellent heat resistance and dimensional stability, typically required for automotive ashtray applications. 04599 is formulated ..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
Solvay Engineered Polymers DEXFLEX® 900 TPO  (discontinued **)
Description: DEXFLEX® 900 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paint..
Linear Mold Shrinkage 0.0082 cm/cm
0.0082 in/in
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..