Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | |
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | |
Plastcom SLOVAMID 6 T 20 PA6, 20% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | Isotropy |
Solvay TECHNYL® A 221 Natural FA PA66, DRY Description: Product in development. Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. Suitable for food contact applicationsAv.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | Isotropy |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | ASTM D955 |
SK Chemicals SKYTHANE® S175A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | ASTM D955 |
Plenco 3356 Phenolic, Granular, Injection Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | ASTM D955 |
Plenco 4599 Phenolic, Granular, Injection Molded PLENCO 04599 is a mineral filled, phenolic molding compound offering excellent heat resistance and dimensional stability, typically required for automotive ashtray applications. 04599 is formulated .. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | |
Solvay Engineered Polymers DEXFLEX® 900 TPO
(discontinued **) Description: DEXFLEX® 900 is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent paint.. |
|||
Linear Mold Shrinkage | 0.0082 cm/cm | 0.0082 in/in | |
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |