Linear Mold Shrinkage 0.0074 - 0.0086 cm/cm
0.0074 - 0.0086 in/in
IS 13411-1992
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..
Linear Mold Shrinkage 0.0070 - 0.0086 cm/cm
0.0070 - 0.0086 in/in
IS 13411-1992
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
Linear Mold Shrinkage 0.0076 - 0.0086 cm/cm
0.0076 - 0.0086 in/in
IS 13411-1992
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium..
Linear Mold Shrinkage 0.0075 - 0.0086 cm/cm
0.0075 - 0.0086 in/in
IS 13411-1992
Amity Thermosets ATG 112 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..
Linear Mold Shrinkage 0.0074 - 0.0086 cm/cm
0.0074 - 0.0086 in/in
IS 13411-1992
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha..