Polymer Property : Linear Mold Shrinkage = 0.0111 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0111 cm/cm
0.0111 in/in
STN EN ISO 294-4
Plastcom PLASTALEN® PQ 81 T 15/1 Polypropylene reinforced with mineral filler, impact modified
Modified PP for injection molding with the content of 15% mineral filler. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.o.
Linear Mold Shrinkage 0.0111 cm/cm
0.0111 in/in
ASTM D955
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0111 cm/cm
0.0111 in/in
STN 64 0808
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant
FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth..
Linear Mold Shrinkage 0.0111 - 0.013 cm/cm
0.0111 - 0.013 in/in
ISO 294
MRC Polymers MAXTELâ„¢ 600T15IMUV TPO, 15% Talc Filled
• For automotive exterior applications• Excellent process ability and dimensional stability• Can be UV Stabilized• Internal and external lubricants can be addedInformation pr..