Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MRC Polymers MAXTELâ„¢ 600T15IMUV TPO, 15% Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer MRC Polymers
Trade Name MAXTEL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MRC Polymers MAXTELâ„¢ 600T15IMUV TPO, 15% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
• For automotive exterior applications• Excellent process ability and dimensional stability• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ISO 1183
Linear Mold Shrinkage 0.0111 - 0.013 cm/cm
0.0111 - 0.013 in/in
ISO 294
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.0 MPa
2320 psi
ISO 527
Flexural Strength 18.0 MPa
2610 psi
ISO 178
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Izod Impact, Notched (ISO) 47.0 kJ/m²
22.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 36.0 °C
96.8 °F
ISO 75
Users viewing this material also viewed the following: