Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.0213 cm/cm | 0.00200 - 0.0213 in/in | Average value: 0.0139 cm/cm Grade Count:39 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |