Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0013 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
ISO 294-4, 2577
Lanxess Durethan® DP 1802 H3.0 000000 Nylon 6
PA 6 injection and extrusion molding grade, non-reinforced, impact-modified, UL 94V-2 off 0,75 mm, GWIT: 775°C off 0,75 mm, halogen-free
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
ISO 294-4, 2577
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6
PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
ISO 294-4, 2577
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber
PBT, 7% glass fibers, injection molding, flame retardant
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Thickness 3.17 mm
0.0013 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Elastoblend® PA6 IM 7040 MB
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro..
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Thickness 3.17 mm
0.0013 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Elastoblend® PA6 IM L
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Thickness 3.17 mm
0.0013 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Elastoblend® PA6 IM L W
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc..
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Thickness 3.17 mm
0.0013 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Elastoblend® PA6 IM X
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat..
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 2955 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2955 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where ..
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface ..
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Thickness 3.17 mm
0.0013 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA6/6 GF7 L 7% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 7% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.0013 - 0.0025 cm/cm

@Time 86400 sec
0.0013 - 0.0025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK
LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.0013 cm/cm
0.0013 in/in
plate with film gate 150x150x3mm<sup>3</sup>
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT
Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou..
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Thickness 2.00 mm
0.0013 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.0013 cm/cm

@Time 86400 sec
0.0013 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP VERTON MV00ASU PP
LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur..
Copyright © lookpolymers.com All Rights Reserved