Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.243 g/cc | 1.243 g/cc | ISO 1183 |
Stir SpA POROCELL EZ 75 S (PVC) Application: Extrusion foam sealInformation provided by STIR SpA |
|||
Specific Gravity | 1.243 g/cc | 1.243 g/cc | |
Hexcel® F161 Epoxy Resin F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is.. |
|||
Specific Gravity | 1.243 g/cc | 1.243 g/cc | |