Polymer Property : Specific Gravity = 1.243 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.243 g/cc
1.243 g/cc
ISO 1183
Stir SpA POROCELL EZ 75 S (PVC)
Application: Extrusion foam sealInformation provided by STIR SpA
Specific Gravity 1.243 g/cc
1.243 g/cc
Hexcel® F161 Epoxy Resin
F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is..
Specific Gravity 1.243 g/cc
1.243 g/cc
Esstech X-744-0000 2-Hydroxyethyl Methacrylate Phosphate, C6H11O6P
HEMA phosphate is a liquid adhesive system that bonds to and interacts with calcium-containing substrates. Listed on the Toxic Substance Control Act List. CAS # 24599-21-1.Information provided by ..