Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers G-04-036ESD PVC Application: High Performance, PVC based compound with antistatic properties. G-04-036ESD is suitable for Gamma radiation sterilization.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers G-3085E PVC Application: General purpose PVC material with good low temperature properties designed for T-Molding extrusion applicationsInformation provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers GA-1050-OR3-LF PVC Application: Lead free, 105° C PVC insulating compound designed for SJEOO applications. Complies with RoHS requirements.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D792 |
S&E Specialty Polymers GR-1409 PVC Application: High flow, high impact rigid PVC based compound. It is suitable for injection molding of the large parts.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D792 |
PTS PBT-1090 PBT Resin Information provided by PTS LLC. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ISO 1183 |
PTS PBT-1100A PBT Resin Information provided by PTS LLC. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D1418 |
Parker Chomerics METALKLIP® Clip-On EMI Gasket Description: Chomerics’ METALKLIP® gasketing is a simple, quick means of mounting on EMI gasket onto 15-20 gauge sheet metal enclosure doors or frames. EMI shielding is provided by either a carbon.. |
|||
Specific Gravity | 1.23 - 1.33 g/cc | 1.23 - 1.33 g/cc | ASTM D 792 |
Karina E CAK 60-48/1 Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina E CAK 65/48/1-CS Black PVC Compound Reclaimed PVC Compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 552-48/1-DT-IE Compound PVC Black PVC Compound for shoe industry with fruit scentInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 552-48/1-DT-IE Compound PVC Black PVC compound for shoe industry with fruit scent.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D 792 |
Karina 600-DA-48/1-C-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina 651-48/1-BY-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina 653D10/1-C-IS White PVC Compound Anti fungus PVC compound for extrusion/drain blow molding.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 18/10-GIN Gray Aluminum MB (SP31454) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 42/234-FC-LMP MB Concentration de Pigment Red for PVC Pigment Concentrate Recommended for Extrusion General PVC. Minimum usage 2%. Organic and Inorganic.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina E 45/28-GEN Gold MB (SP31471) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina E 48/23-RG-PO Black Color Concentrate for PVC Color concentrate in powder form recommended for application in PVC compounds for general purposes extrusion and injection. Recommended to use 2%.Information provided by Karina Indústria e ComÃ.. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina E 630-10/175-A-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina 40/272-FC-LMP Green Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | ASTM D 792 |
Karina E 858-10/16-ERYA PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 1522 Wire & Cable Flexible PVC Vinyl elastomer jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 18760 Wire & Cable Flexible PVC Non-lead stabilized, matte-finish, jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil. Ideally suited for 90°C applications.Information p.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | Dipping/distilled water; ISO 1183 |
BLUESTAR PBT 1100 PBT resin is polymerized by pure terephthalic acid (PTA) and 1,4-butanediol (1,4-BDO) through direct esterification. With well-distributed molecular weight and stable quality, PBT resin possesses go.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 21572 Coax & Telecom Flexible PVC Semi-rigid non-lead stabilized insulation compound designed for data communication riser cable applications. Maximum 60°C service temperature rating.Information provided by Georgia GulfGeorgia Gul.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 22561 Coax & Telecom Flexible PVC Non-lead stabilized, semi-rigid insulation compound for minimum transmission interference in communication applications. Suitable for use as a riser insulation.Information provided by Georgia GulfG.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 50896 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 19732 Wire & Cable Flexible PVC Non-lead stabilized, electrical grade 105°C rated non-lead vinyl elastomer compound suitable for SEO and SJEO insulation and jacket applications per UL 62.Information provided by Georgia GulfGeorgi.. |
|||
Specific Gravity | 1.29 - 1.33 g/cc | 1.29 - 1.33 g/cc | ASTM D-792 |
Axiall 4590 Flexible PVC 10 mil automotive thin wall insulation.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.27 - 1.33 g/cc | 1.27 - 1.33 g/cc | NBR NM-IEC 60811-1-3 |
Karina 39/32-GI Pink Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |