Parker Chomerics METALKLIP® Clip-On EMI Gasket

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name METALKLIP®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics METALKLIP® Clip-On EMI Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chomerics’ METALKLIP® gasketing is a simple, quick means of mounting on EMI gasket onto 15-20 gauge sheet metal enclosure doors or frames. EMI shielding is provided by either a carbon-filled silicone strip or by monel (nickel-copper alloy) over silicone strip. A non-standard alternative is Ferrex wire over neoprene. The gasket is secured in a corrosion-resistant, stainless steel spring clip. No holes or fasteners are required for installation. Integral sharp teeth on the clip bite through paint or surface oxides to provide electrical continuity from gasket to chassis.Mesh Over Core:Monel Wire: 0.0035 in. (0.09 mm) diameter per QQ-N-281, 2 layers.Silicone Tube: ZZ-R-765Clip: Stainless steel, 0.02 in. (0.51 mm) thick, series 302/305Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.27 - 1.33 g/cc
1.27 - 1.33 g/cc
ASTM D1418
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 70
60 - 70
ASTM D2240
Tensile Strength >= 2.76 MPa
>= 400 psi
ASTM D412
Elongation at Break >= 150 %
>= 150 %
ASTM D412
Tear Strength >= 8.77 kN/m
>= 50.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 10 ohm-cm
<= 10 ohm-cm
ASTM D991
Descriptive Properties Value Comments
Color Black