Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.35 - 1.65 g/cc | 1.35 - 1.65 g/cc | |
Parker Chomerics CHO-SHIELD® 4900 Conductive Coating CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Fil.. |
|||
Specific Gravity | 1.55 - 1.65 g/cc | 1.55 - 1.65 g/cc | ASTM D1475 |
Lotus Nano Paint NAX 01P Tow-Component Nano-paint Description: More durable and specific application methods. This paint is suitable for traffic signs on the road, cross-walks, warning vibrating lines and limited lot marking. Related machines could.. |
|||
Specific Gravity | 1.59 - 1.65 g/cc | 1.59 - 1.65 g/cc | ASTM D 792 |
Karina 837-38/29-E-ERYB Straw PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall EX 3154 Plenum Flexible PVC Non-lead stabilized CAT 3 plenum jacket. Recommended for up to 25 pair, unshielded.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall H 5126A Plenum Flexible PVC Plenum-grade Cat-5(+) jacket for use over 100% FEP. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall H 5177B Plenum Flexible PVC Plenum-grade jacket with good low temperature properties for use over 100% FEP primaries. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall 02541 Plenum Flexible PVC Non-lead stabilized CAT 3 jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall 1275 Plenum Flexible PVC Plenum-grade optical fiber jacket. UL QMTM2 recognized component for plenum cable compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.55 - 1.65 g/cc | 1.55 - 1.65 g/cc | Natural; ASTM D-792 |
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit.. |
|||
Specific Gravity | 1.59 - 1.65 g/cc | 1.59 - 1.65 g/cc | ASTM D 792 |
Karina 802-18/462-C-ERB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |