Axiall Tuf-Stif 2804 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name Tuf-Stif
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall Tuf-Stif 2804 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidity/StiffnessDimensional StabilityDurabilityColorabilityFlame retardantChemical ResistanceInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.55 - 1.65 g/cc
1.55 - 1.65 g/cc
Natural; ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM D-638
Tensile Modulus 4.14 GPa
600 ksi
ASTM D-638
Flexural Strength 86.2 MPa
12500 psi
ASTM D-790
Flexural Modulus 4.65 GPa
675 ksi
ASTM D-790
Izod Impact, Notched 0.534 J/cm

@Temperature 23.0 °C
1.00 ft-lb/in

@Temperature 73.4 °F
ASTM D-256
Thermal Properties Metric English Comments
CTE, linear 37.8 µm/m-°C

@Temperature 20.0 °C
21.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D-648
Flammability, UL94 V-0
V-0
At 0.125 inch(pending)
Processing Properties Metric English Comments
Zone 1 149 °C
300 °F
Zone 2 154 °C
310 °F
Zone 3 160 °C
320 °F
Zone 4 166 °C
330 °F
Zone 5 171 °C
340 °F
Die Temperature 179 °C
355 °F
Melt Temperature 188 - 199 °C
370 - 390 °F