Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.757 g/cc | 1.757 g/cc | as shipped |
Imerys KT Cast Slurryâ„¢ Kaolin KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys |