Polymer Property : Specific Gravity = 1.757 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.757 g/cc
1.757 g/cc
as shipped
Imerys KT Cast Slurryâ„¢ Kaolin
KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys