Greene Tweed CHEMRAZ® 655 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 655 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz® 655 is Greene Tweed’s high-temperature off-white perfluoroelastomer. Specifically developed for wafer processes with operating temperatures up to 315°C (600°F), Chemraz 655 provides excellent chemical resistance with minimal particle generation. Available in a wide range of geometries and cross sections, this material offers the diversity required for a variety of dynamic or static dry processing applications.Applications:Door sealsSlit valvesWindow sealsIsolator valve sealsLid sealsGas inlet sealsKF fitting sealsChamber sealsValve sealsEndpoint windowsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.11 g/cc
2.11 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength at Break 12.9 MPa
1870 psi
ASTM D1414
Tensile Strength, Yield 4.14 MPa
600 psi
@50% Elongation; ASTM D1414
7.17 MPa
1040 psi
@100% Elongation; ASTM D1414
Elongation at Break 190 %
190 %
ASTM D1414
Compression Set 15 %
15 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 316 °C
600 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Descriptive Properties Value Comments
Color Off-White