Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ISO 12086 |
Isoflon FEP Fluorinated Ethylene Propylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Specific Gravity | 2.15 - 2.17 g/cc | 2.15 - 2.17 g/cc | |
Shandong Dongyue Shenzhou New Material Co DS601 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-230ASL PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for extrusion molded parts. Piping, tube, etc... |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-210 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided .. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Specific Gravity | 2.14 - 2.17 g/cc | 2.14 - 2.17 g/cc | ASTM D792 |
Adamas Adalon® 902 PTFE, 1% Conductive filler Information provided by Adamas, HPM |
|||
Specific Gravity | 2.15 - 2.17 g/cc | 2.15 - 2.17 g/cc | ASTM D792 |
Adamas Adalon® 992 Modified PTFE Information provided by Adamas, HPM |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-66P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-802UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ISO 12086 |
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Specific Gravity | 2.14 - 2.17 g/cc | 2.14 - 2.17 g/cc | |
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |