Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.12 g/cc | 2.12 g/cc | ASTM D1505 |
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Specific Gravity | 2.12 g/cc | 2.12 g/cc | ASTM D1505 |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Specific Gravity | 2.12 g/cc | 2.12 g/cc | ASTM D792 |
Greene Tweed Avalon® 9 PTFE, Graphite Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Specific Gravity | 2.12 g/cc | 2.12 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 534 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D-792 |
Saint-Gobain Norton® FEP Fluoropolymer Film Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp.. |
|||
Specific Gravity | 2.12 - 2.18 g/cc | 2.12 - 2.18 g/cc | ASTM D-792 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-210AS PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Anti-static grader for injection molding.Information provided by D.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-201 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Complicated injection molded parts requiring high melt flow to fil.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-210 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Injection molded parts, wire insulation, etc.Information provided .. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | at 25°C |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-65P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-802UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Asahi Glass Fluon® P-830UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc | ISO 12086 |
Isoflon MFA TFE/Perfluoromethylvinylether Copolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Specific Gravity | 2.12 - 2.20 g/cc | 2.12 - 2.20 g/cc | ASTM D792 |
Adamas Adalon® 911 PTFE Information provided by Adamas, HPM |