Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 151000 cP @Shear Rate 500 1/s, Temperature 295 °C |
151000 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m.. |
|||
Viscosity | 151000 cP @Shear Rate 5000 1/s, Temperature 200 °C |
151000 cP @Shear Rate 5000 1/s, Temperature 392 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AF is a high viscosity acetal homopolymer containing 20% Teflon PTFE fibers. It is designed for a.. |