Polymer Property : Linear Mold Shrinkage, Transverse = 0.0058 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
Plastcom SLOVAMID 6 GF 30 FRGG2 PA6, 30% glass fibre, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
STN EN ISO 294-4
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded
PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the ..
Linear Mold Shrinkage, Transverse 0.0058 cm/cm

@Time 86400 sec
0.0058 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compounding
Linear Mold Shrinkage, Transverse 0.0058 cm/cm

@Thickness 2.00 mm
0.0058 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6  (Unverified Data**)
Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided ..
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 30 EF 000000 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, low viscosity (Easy Flow)
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
60x60x2; 280°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber
PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
ASTM D955
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p..
Linear Mold Shrinkage, Transverse 0.0058 - 0.0059 cm/cm

@Time 86400 sec
0.0058 - 0.0059 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC
LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable.
Linear Mold Shrinkage, Transverse 0.0058 cm/cm
0.0058 in/in
ISO 294
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.