Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0083 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0083 cm/cm
0.0083 in/in
Plastcom SLOVAMID 6 GF 15 FRG 2 LW PA6, 15% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fibre, with nonhalogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 960°..
Linear Mold Shrinkage, Transverse 0.0083 cm/cm

@Thickness 3.00 mm
0.0083 in/in

@Thickness 0.118 in
Mold Temp 80°C; Melt Temp 280°C; 400 bar; ISO 294-4
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers
PA 6-Copolymer, 15% glass fibers, injection molding, impact modified
Linear Mold Shrinkage, Transverse 0.0083 cm/cm
0.0083 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific)
LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0083 cm/cm

@Time 86400 sec
0.0083 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific)
LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0083 cm/cm
0.0083 in/in
ISO 294-4
DSM Akulon® K224-G8 PA6-GF40
40% Glass Reinforced
Linear Mold Shrinkage, Transverse 0.0083 cm/cm
0.0083 in/in
60x60x2 mm; ISO 294
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
Linear Mold Shrinkage, Transverse 0.0083 cm/cm
0.0083 in/in
ISO 294-4
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Linear Mold Shrinkage, Transverse 0.0083 cm/cm

@Time 86400 sec
0.0083 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated.