Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
STN 64 0808
Plastcom SLOVAMID 6 FRC 2 Polyamide 6, Halogen Free Flame Retardant
FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electro-technical purposes. Excellent flow of the material predetermines..
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
Plastcom SLOVAMID 6 FRC 3 PA6, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 for injection moulding with increased flammability resistance, with nonhalogen and phosporus flame retardant. Excellent..
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 30 FRG 5 Polyamide 6, 30% Glass Fiber, Halogen Free Flame Retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,..
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent..
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength
FeaturesChemically reinforced with 14% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I..
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
STN EN ISO 294-4
Plastcom SLOVAMID® 6/66 FRC 3 TS PA6/66 flame retarded, heat stabilized
PA 6 + PA 66 alloy for injection molding, reinforced with 30 % glass fiber, flame retarded with non halogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 5 a..
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage, Transverse 0.0087 - 0.0107 cm/cm

@Time 86400 sec
0.0087 - 0.0107 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12
4.3 specific gravity nylon 12, clean compound system
Linear Mold Shrinkage, Transverse 0.0087 cm/cm
0.0087 in/in
Plastcom SLOVAMID 6 FRC 2 TS PA6, flame retardant, heat stability
FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre..
Linear Mold Shrinkage, Transverse 0.0087 cm/cm

@Time 86400 sec
0.0087 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.