Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm

@Thickness 1.00 mm
0.0060 - 0.0080 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm

@Thickness 1.00 mm
0.0040 - 0.0080 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm

@Thickness 3.00 mm
0.0060 - 0.0080 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm

@Thickness 3.00 mm
0.0060 - 0.0080 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm

@Thickness 3.00 mm
0.0050 - 0.0080 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm

@Thickness 1.00 mm
0.0040 - 0.0080 in/in

@Thickness 0.0394 in
Absolute Drying
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm

@Thickness 3.00 mm
0.0040 - 0.0080 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® TY-145TZ Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm

@Thickness 3.00 mm
0.0050 - 0.0080 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm

@Thickness 1.00 mm
0.0060 - 0.0080 in/in

@Thickness 0.0394 in
DAM
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm

@Thickness 1.00 mm
0.0060 - 0.0080 in/in

@Thickness 0.0394 in
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0080 in/in

@Thickness 0.125 in
Direction of Flow; ASTM D955
Diamond Polymers Softflex® 6538 Thermoplastic Elastomer Alloy, Clear
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0080 in/in

@Thickness 0.125 in
Transverse to Flow; ASTM D955
Diamond Polymers Softflex® 6538 Thermoplastic Elastomer Alloy, Clear
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm

@Thickness 3.00 mm
0.0050 - 0.0080 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..