Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.017 - 0.020 cm/cm

@Thickness 3.20 mm
0.017 - 0.020 in/in

@Thickness 0.126 in
Flow, 24h; ASTM D955
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
Linear Mold Shrinkage 0.017 - 0.020 cm/cm

@Thickness 3.20 mm
0.017 - 0.020 in/in

@Thickness 0.126 in
Transverse, 24h; ASTM D955
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
Linear Mold Shrinkage 0.017 - 0.020 cm/cm

@Thickness 3.17 mm
0.017 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.018 - 0.020 cm/cm

@Thickness 3.17 mm
0.018 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 4115-104D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 3015-201 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.015 - 0.020 cm/cm

@Thickness 3.00 mm
0.015 - 0.020 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.017 - 0.020 cm/cm

@Thickness 3.20 mm
0.017 - 0.020 in/in

@Thickness 0.126 in
Transverse, 24h; ASTM D955
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer
Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 3015-104 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 4115-201D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..