Polymer Property : Melt Index of Compound = 44 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 44 g/10 min

@Load 2.16 kg,
Temperature 230 °C
44 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Dow C705-44NA Polypropylene Impact Copolymer Resin
DOW C705-44NA Polypropylene Resin is a high melt flow rate impact copolymer that combines superior stiffness and good impact resistance. The product is intended for use in injection molding applica..
Melt Index of Compound 44 g/10 min

@Load 2.16 kg,
Temperature 190 °C
44 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow DMDA-8940 NT 7 High Density Polyethylene Resin
DOW DMDA-8940 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info..
Melt Index of Compound 44 g/10 min

@Load 2.16 kg,
Temperature 250 °C
44 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm3/10 min; ISO 1133
DuPont Performance Polymers Crastin® S610SF NC010 PBT  (Unverified Data**)
Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati..