Material Notes:
Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.017 cm/cm
0.017 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4
Melt Index of Compound 44 g/10 min

@Load 2.16 kg,
Temperature 250 °C
44 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm3/10 min; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa

@Temperature 23.0 °C
8120 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 40 %

@Temperature 23.0 °C
40 %

@Temperature 73.4 °F
nominal; ISO 527
Elongation at Yield 4.0 %

@Temperature 23.0 °C
4.0 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 2.50 GPa

@Temperature 23.0 °C
363 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 240 °C
464 °F
Optimum; Injection Molding
235 - 260 °C
455 - 500 °F
Injection Molding
Mold Temperature 80.0 °C
176 °F
optimum; Injection Molding
30.0 - 130 °C
86.0 - 266 °F
Injection Molding
Drying Temperature 110 - 130 °C
230 - 266 °F
Injection Molding
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Injection Molding
Moisture Content <= 0.040 %
<= 0.040 %
Injection Molding
Descriptive Properties Value Comments
Appearance Natural Color
Drying Recommended Yes
Injection Molding
Features Chemical Resistance, Good
Dimensional Stability, Good
Flow, High
Moisture Absorption, Low
Molding Cycle, Fast
Processability, Good
Viscosity, Low
Forms Pellets
Generic PBT
Material Status Preliminary Data
Part Marking Code >PBT<
ISO 11469
Processing Method Injection Molding
Product Category Fast Cycle Resins
Fast Cycle Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification PBT
ISO 1043
RoHS Compliance Contact Manufacturer
Users viewing this material also viewed the following: