Physical Properties Metric English Comments
Viscosity 155 - 185 cP

@Temperature 30.0 °C
155 - 185 cP

@Temperature 86.0 °F
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer
Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo..
Viscosity 155 - 185 cP

@Temperature 30.0 °C
155 - 185 cP

@Temperature 86.0 °F
3D Systems Accura® 55 Plastic for SLA® Systems
Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic compon..
Viscosity 155 cP

@Temperature 25.0 °C
155 cP

@Temperature 77.0 °F
BASF Pluracol® 1203 Specialty Polyol
Description: Pluracol® 1203 is a conventional polyol with 2- and 3-functional characteristics. Pluracol1203 is specially designed for 1-component adhesives, foam-sealants, and microcellular elasto..