Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 155 - 185 cP @Temperature 30.0 °C |
155 - 185 cP @Temperature 86.0 °F |
|
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo.. |
|||
Viscosity | 155 - 185 cP @Temperature 30.0 °C |
155 - 185 cP @Temperature 86.0 °F |
|
3D Systems Accura® 55 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic compon.. |