Polymer Property : Viscosity = 15500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 15500 cP

@Temperature 25.0 °C
15500 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Bond 2106 Fast Cure, Medium Viscosity Epoxy Adhesive
TRA-BOND 2106 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This clear, two-part, medium viscosity syste..
Viscosity 15500 cP
15500 cP
mixing, dynamic
Dow Corning SILASTIC® 3497 MOULD MAKING BASE & 96 CURING AGENT
High strength, low hardness, fast cure silicone mold making rubber featuring a very good resistance to polyester resin and suited for the detailed reproduction of fiines, art objects and similar ite..
Viscosity 15500 cP
15500 cP
Mixed; TM R050-12
Resinlab® EP1026 Clear Epoxy Adhesive
Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..
Viscosity 15500 cP
15500 cP
Mixed; TM R050-12
Resinlab® EP1026 Black Epoxy Adhesive
Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..