Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 15500 cP @Temperature 25.0 °C |
15500 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2106 Fast Cure, Medium Viscosity Epoxy Adhesive TRA-BOND 2106 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This clear, two-part, medium viscosity syste.. |
|||
Viscosity | 15500 cP | 15500 cP | mixing, dynamic |
Dow Corning SILASTIC® 3497 MOULD MAKING BASE & 96 CURING AGENT High strength, low hardness, fast cure silicone mold making rubber featuring a very good resistance to polyester resin and suited for the detailed reproduction of fiines, art objects and similar ite.. |
|||
Viscosity | 15500 cP | 15500 cP | Mixed; TM R050-12 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Viscosity | 15500 cP | 15500 cP | Mixed; TM R050-12 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |