Polymer Property : Viscosity = 2900 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2300 - 2900 cP

@Shear Rate 1.00 1/s,
Temperature 25.0 °C
2300 - 2900 cP

@Shear Rate 1.00 1/s,
Temperature 77.0 °F
LVF#4, Uncured
Fibre Glast 182 White Gel Coat
#182 White Gel Coat is a highly durable ISO gel coat and is the industry production standard for molding applications. Use as a sandable base coat for painting or polish to a high luster finish. Spr..
Viscosity 1900 - 2900 cP
1900 - 2900 cP
Cone & Plate; ISO 3219 (93)
Dow SPECFLEX™ NC 606 Polyol
SPECFLEX™ NC 606 polyol is a co-polymer polyol especially designed for the production of High Resilience (HR) molded flexible foams. It processes well on all types of foam machinery. CAS# 00908..
Viscosity 1900 - 2900 cP

@Temperature 35.0 °C
1900 - 2900 cP

@Temperature 95.0 °F
C.O.I.M. UREXTER® T 400 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Viscosity 2500 - 2900 cP
2500 - 2900 cP
15% solution in MEK
Lubrizol Advanced Materials Pearlstick® 46-73/27 Polyester based TPU  (discontinued **)
TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa