Physical Properties Metric English Comments
Viscosity 2.5 cP
2.5 cP
ASTM D2196
Parker Chomerics THERM-A-FORM T642 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Viscosity 2.5 cP
2.5 cP
ASTM D2196
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..