Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 255000 cP @Temperature 240 °C |
255000 cP @Temperature 464 °F |
melt; 1000 sec-1; ASTM D 3825 |
SABIC Innovative Plastics Cycolac® MG37CR ABS High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Viscosity | 255000 cP @Temperature 240 °C |
255000 cP @Temperature 464 °F |
melt; 1000 sec-1; ASTM D 3825 |
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific) High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Viscosity | 255000 cP @Temperature 260 °C |
255000 cP @Temperature 500 °F |
melt; 1000 sec-1; ASTM D 3825 |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Viscosity | 255000 cP @Temperature 260 °C |
255000 cP @Temperature 500 °F |
melt; 1000 sec-1; ASTM D 3825 |
SABIC Innovative Plastics Cycolac® Z48 ABS Automotive. Very high heat resistance with medium impact and good strength properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Viscosity | 255000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
255000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® T85 SG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Hig.. |
|||
Viscosity | 255000 cP @Shear Rate 300 1/s, Temperature 190 °C |
255000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2160 NC Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |
|||
Viscosity | 255000 - 255000 cP @Temperature 240 - 240 °C |
255000 - 255000 cP @Temperature 464 - 464 °F |
Average value: 255000 cP Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |