Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 225000 - 255000 cP @Temperature 260 - 260 °C |
225000 - 255000 cP @Temperature 500 - 500 °F |
Average value: 245000 cP Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Viscosity | 255000 - 255000 cP @Temperature 240 - 240 °C |
255000 - 255000 cP @Temperature 464 - 464 °F |
Average value: 255000 cP Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |