Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 180 - 260 cP | 180 - 260 cP | |
LG Chemical CP-ST Advantage: Super slump retention; Low concrete viscosity; Good combination with water reducer (WRM, WB, RS)Main Uses: Super slump retentionInformation provided by LG Chemical |
|||
Viscosity | 45.0 - 260 cP | 45.0 - 260 cP | Average value: 148 cP Grade Count:3 |
Overview of materials for Chlorosulfonated Polyethylene Rubber This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val.. |