Viscosity 10000 - 26000 cP
10000 - 26000 cP
Lord Adhesives 202 Semi-Flexible, Fast Cure, Medium Viscosity Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..
Viscosity 22000 - 26000 cP

@Temperature 23.0 °C
22000 - 26000 cP

@Temperature 73.4 °F
10 rpm
Epoxy Technology EPO-TEK® E3037 Epoxy
Material Description: A single component, electrically conductive, thixotropic silver-filled epoxy for die-attach and SMD-attach inside hybrid microelectronics.Information Provided by Epoxy Technolo..
Viscosity 22000 - 26000 cP

@Temperature 23.0 °C
22000 - 26000 cP

@Temperature 73.4 °F
10 rpm
Epoxy Technology EPO-TEK® H37-MP Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H37-MP is a single component, electrically conductive, thixotropic silver-filled adhesive for die-attach and SMD attach inside hybrid microelectronic packages. Also av..
Viscosity 24000 - 26000 cP
24000 - 26000 cP
uncured
Atom Adhesives AA-BOND FDA2T Epoxy Adhesive
AA-BOND FDA2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received ..