Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 27000 - 30000 cP | 27000 - 30000 cP | |
Master Bond EP46HT-1 Epoxy For Serviceability Up To 600°F Description: Master Bond EP46HT-1 is a two component epoxy system for high performance structural bonding and sealing suitable for applications where resistance to temperatures from -100°F to +550°.. |
|||
Viscosity | 27000 cP @Temperature 25.0 °C |
27000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond CA20 Coil-Fix Epoxy Adhesive TRA-BOND CA-20 is a thixotropic epoxy adhesive system specially formulated for shorted turns, damaged end wire extensions, or other coil repair applications where a high-fill, non-sag adhesive is re.. |
|||
Viscosity | 27000 cP @Temperature 25.0 °C |
27000 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy TRA-DUCT 916D01 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr.. |
|||
Viscosity | 27000 cP | 27000 cP | |
Dymax 910 Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 910 Strain Relief, Wire and Parts Tacking AdhesiveFlexible, good adhesion and mechanical removable Cure Type: UV |
|||
Viscosity | 27000 cP | 27000 cP | uncured |
Atom Adhesives AA-BOND FDA22 Epoxy Adhesive AA-BOND FDA22 is a high viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administ.. |
|||
Viscosity | 27000 cP | 27000 cP | |
ACC MM913 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |