Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 42 cP @Temperature 25.0 °C |
42 cP @Temperature 77.0 °F |
of Solution, 5% wt/wt in Styrene |
Polimeri Europa Intene® C 30 AF Butadiene Rubber Intene® C 30 AF is a solution polymerized low cis polybutadiene produced using an alkyl lithium catalyst. A TNPP free, food contact approved, non-staining antioxidant is added during the productio.. |
|||
Viscosity | 42 - 52 cP | 42 - 52 cP | |
Huntsman Araldite DY 3601 Reactive Diluent Weight per Epoxide (EEW, g/eq) 385 to 405. Max color is 3.Comments/Applications: Low viscosity, polypropylene glycol-based epoxy resin. Enhances flexibility and impact resistance.Data provided by .. |
|||
Viscosity | 42 cP @Temperature 30.0 °C |
42 cP @Temperature 86.0 °F |
5% wt Toluene Solution |
Kuraray SEPTON® S8006 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Viscosity | 42 cP | 42 cP | 5% Styrene solution; NM-300-32 |
Dynasol Solprene® 1106 Solution Styrene-Butadiene Rubber (SSBR) Solprene® 1106 is a linear high molecular weight random-block styrene/butadiene copolymer with 10% styrene, 6% present as a polystyrene block. This grade has a non-staining antioxidant system; FDA.. |