Polymer Property : Viscosity = 52 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 42 - 52 cP
42 - 52 cP
Huntsman Araldite DY 3601 Reactive Diluent
Weight per Epoxide (EEW, g/eq) 385 to 405. Max color is 3.Comments/Applications: Low viscosity, polypropylene glycol-based epoxy resin. Enhances flexibility and impact resistance.Data provided by ..