Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 6000 cP @Temperature 190 °C |
6000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 3460 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Component of modified bitum.. |
|||
Viscosity | 6000 cP @Temperature 190 °C |
6000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 4460 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Wire and Cable fillings and flooding .. |
|||
Viscosity | 6000 - 8000 cP | 6000 - 8000 cP | |
ND Industries 446 High pressure Sealant Very high strength refrigerant sealant. Maximum solvent resistance |
|||
Viscosity | 6000 - 8000 cP | 6000 - 8000 cP | |
ND Industries StudGrade® 137 Permanent HT Threadlocker General DescriptionHigh strength, high temperature threadlockers for heavy duty applications. Suitable for most applications where disassembly is not required. |
|||
Viscosity | 6000 cP | 6000 cP | mix viscosity |
Aremco Aremco-Bond™ 855 Epoxy Adhesive
(discontinued **) High performance epoxy for specialty bonding and potting applications to 350ºF (175°C). Can be applied to a myriad of substrates, offering exceptional chemical, electrical, and mechanical properti.. |
|||
Viscosity | 6000 - 40000 cP | 6000 - 40000 cP | |
Huntsman Araldite GZ 540 X-90 Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 233 to 278. Max color is 3.Comments/Applications: GY 6040 - 90% solids in xylene. General purpose bis A epoxy solution for use in 2-package maintenance and architect.. |
|||
Viscosity | 6000 - 7000 cP @Temperature 23.0 °C |
6000 - 7000 cP @Temperature 73.4 °F |
|
Master Bond EP41S-1 Chemically Resistant Two Component Epoxy System Master Bond Polymer System EP41S-1 is a two component epoxy resin system designed for durable, high performance
bonding, sealing, coating and encapsulating. It successfully withstands prolonged imm.. |
|||
Viscosity | 6000 - 6500 cP | 6000 - 6500 cP | mixed |
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre.. |
|||
Viscosity | 6000 - 10000 cP @Temperature 23.0 °C |
6000 - 10000 cP @Temperature 73.4 °F |
|
Master Bond UV15-7LRI One Component, Optically Clear UV Curable System Master Bond Polymer System UV15-7LRI is a one component, optically clear, non-yellowing UV curable polymer system for high performance adhesives, sealants and coatings. When exposed to a source of U.. |
|||
Viscosity | 6000 cP | 6000 cP | Dynamic |
Dow Corning XIAMETER® PMCPOHX-4012 Polymer 6000CS Is chemically equivalent to DOW CORNING® 3-0113 POLYMER. OH end-blocked polydimethylsiloxane, viscosity 6,000 cP, OH/Silanol content 1,300ppm.Information provided by Dow Corning |
|||
Viscosity | 6000 cP | 6000 cP | dynamic |
Dow Corning 1520-US ANTIFOAM Dow Corning Antifoam 1520-US was specifically formulated for food contact applications.Information provided by Dow Corning |
|||
Viscosity | 6000 cP | 6000 cP | |
Dymax 3094 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 6000 cP | 6000 cP | |
Dymax 9-984-B Conformal Coating High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-984-B Conformal CoatingCures to an opaque black finish; hides components or circuitry from view; protects sensitiv.. |
|||
Viscosity | 6000 cP | 6000 cP | |
ACC MM820 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 6000 cP | 6000 cP | "B" component |
ACC QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Viscosity | 6000 - 12000 cP | 6000 - 12000 cP | |
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |
|||
Viscosity | 6000 cP | 6000 cP | |
Aremco Crystalbond™ 509 Washaway Mounting Adhesive & Accessory Provides excellent adhesion and minimizes clogging of diamond tools compared to waxes. Transparent in thin cross-sections. Soluble in acetone or 509-S stripper, an odorless, non-flammable, biodegrad.. |
|||
Viscosity | 6000 cP @Temperature -20.0 °C |
6000 cP @Temperature -4.00 °F |
Cold Crank |
ChevronTexaco URSA® SAE 10W-30 Super Plus Texaco Ursa Super Plus SAE 10W-30 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.Reduced inventory investment — No need to maintai.. |
|||
Viscosity | 6000 - 12000 cP | 6000 - 12000 cP | Accelerator |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |
|||
Viscosity | 6000 cP | 6000 cP | Part B, RVT, #6, 20 rpm; TM R050-12 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |